A metal powder contains not less than 0.10 mass % and not more than 1.00 mass % of at least one of chromium and silicon, and a balance of copper. The total content of the chromium and the silicon is not more than 1.00 mass %. In accordance with an additive manufacturing method for this metal powder, an additively-manufactured article made from a copper alloy is provided. The additively-manufactured article has both an adequate mechanical strength and an adequate electrical conductivity.

A method of forming an additively manufactured aluminum part includes establishing an arc between a metal-cored aluminum wire and the additively manufactured aluminum part, wherein the metal-cored aluminum wire includes a metallic sheath and a granular core disposed within the metallic sheath. The method includes melting a portion of the metal-cored aluminum wire using the heat of the arc to form molten droplets. The method includes transferring the molten droplets to the additively manufactured aluminum part under an inert gas flow, and solidifying the molten droplets under the inert gas flow to form deposits of the additively manufactured aluminum part.

A forming apparatus having a degree of freedom in shaping for forming a three-dimensional structure is provided. A forming apparatus (30) forms a three-dimensional structure (5), which includes a shaped article and a colored portion that colors a surface of the shaped article, by laminating layers, and it can switch between a first operation mode dedicated to shaping the shaped article and a second operation mode of full-color coloring the surface of the shaped article using full colors simultaneously as the shaping of the shaped article.

Explore More Patents

Discover additional patents in the cpc category

Browse All Patents